Features:
- Small coefficient of heat conductivity and good capability of heating preservation, outstanding effect of energy-saving.
- Excellent fireproof capability.
- Excellent sound absorption and sound insulation capability.
- Stable capability of chemistry may keep the long-term using.
- No causticity effects the heat preservation materials.
- Green building materials and no harm for body.
- Broad using range.
Technical Performance:
Product |
Density (kg/m3) |
Thickness (mm) |
Length (mm) |
Width (mm) |
Rock wool slab |
60 |
50-80 |
1200 |
600 |
80 |
40-100 |
1000 |
630 |
100 |
30-100 |
120 |
40-80 |
150 |
40-60 |
180 |
40-60 |
Rock wool felt |
80 |
50-100 |
3000 |
910 |
100 |
40-100 |
Rock wool pipe section |
130 |
30-80 |
1000 |
18-350 |
Physical Performance:
Item |
Testing Result |
Standard |
Density Tolerance (%) |
8.3 |
±15 |
Binder content (%) |
2.9 |
≤4.0 |
Working temperature (℃) |
600 |
≥600 |
Thermal conduct w/(m·k)(70±5℃) |
0.04 |
≤0.044 |
Combustion |
Non-combustible |
Non-combustible |
Average Fiber Diameter (ūm) |
5.7 |
≤7.0 |
Slag Nodule Content (%) |
4.2 |
≤12.0 |
CIˉ |
0.0058 |
--- |
Thermal Insulation for Equipment and Pipes:
Types Properties |
Slab |
Faced Stitched Mat |
Pipe Section |
Density (kg/m3) |
60-180 |
80-120 |
100-150 |
Thermal conduct equation (w/m·k) |
0.035+0.00018 tm |
0.028+0.00023 tm |
0.036+0.00015 tm |
Working temperature ℃ |
600 |
600 |
600 |
Application field |
Equipment with plane or big curve surface |
Equipment and big diameter pipes |
Pipes with small diameter |
Chemical Composition:
Chemical Item |
Testing Result (%) |
Chemical Item |
Testing Result(%) |
SiO2 |
42.21 |
MnO |
0.31 |
Al2O3 |
11.88 |
Na2O |
0.33 |
CaO |
33.41 |
TiO2 |
0.81 |
MgO |
9.24 |
K2O |
0.65 |
Fe2O3 |
0.78 |
- |
Physical-chemical Performance:
Item |
Testing Result |
Standard Result |
Volume density(kg/m3) |
148 |
≤240 |
Averaged fiber diameter(mm) |
4.8 |
≤5.0 |
Water ratio(%) |
0.03 |
≤0.20 |
Organic matter content(%) |
0.13 |
≤0.30 |
Fiber strength(WT value mm) |
65.3 |
≥50 |
Acidity coefficient |
1.27 |
≥1.10 |
Grain size distribution(%)(>12mm) |
95.3 |
≥20.0 |
Slag particle content(%)(single diameter>0.5mm) |
0.3 |
≤2.0 |
Slag particle summation(%) |
24.7 |
≤25.0 |
Heat shrinkage temperature(℃) |
702 |
--- |
Combustibility |
Non-combustible |
Non-combustible |
Thermal Coefficient:
Inspection Item |
Experiment Method |
W/(m·K) Measured Result |
Average Temperature 50 ℃ |
GB/T10294-1988 |
0.042 |
Average Temperature 102 ℃ |
0.046 |
Average Temperature 151℃ |
0.053 |
Average Temperature 200℃ |
0.058 |
Average Temperature 250 ℃ |
0.064 |
Average Temperature 301 ℃ |
0.073 |
Average Temperature 350 ℃ |
0.08 |
Average Temperature 400 ℃ |
0.086 |
Construction Requirement:
1.The consistency standards of the rock wool slab used 150kg per m3 above, and the intensity of pressure resistance of the slab of 150kg per m3 is equals to or more than 40KN per m2; and the intensity of pressure resistance of the slab of 180kg per m3 is equals to or more than 60KN per m2.
2.To achieve the best effect of heat preservation, double-layer rock wool slab need to lay in the break joint.
3.In the process of fixing the materials of heat preservation and waterproofing, or dealing with the gutter inlet, the special.
4.Fittings needed lo prevent water from contacting the rock wool slab directly.